Microstructured electrodes supported on serpentine ...
2019-2-22 · Then, the composite powder was mixed with N-methyl-2-pyrrolidone (NMP) to obtain a paste that was doctor bladed on top of the aluminum foil. The electrode was dried under vacuum at 110 °C for 12 h to achieve a LNMO composite electrode thickness of 100 μm.